Determination of Bond Work Index of Lucky Cement
Ball mill was employed to conduct the grinding test of seven different samples. Among all seven samples collected from the different faces of quarry, Bond work index of limestone Face4A results less than 20kwh/t, remaining 6 samples are marked as hard rock because of